Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Ultramid® B35G3 BK00564 - PA6-GF15 - BASF

Material Data Center offers the following functions for Ultramid® B35G3 BK00564:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Ultramid B datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
材料文字说明
Glass fibre reinforced injection moulding grade e.g. for internal gas pressure applications such as steering column switch, automobile mirror housings and wheels of mountain bikes.
机械性能干 / 已调节单位Test Standard
ISO数据
拉伸模量 6100 / 3200 MPa ISO 527
断裂应力 126 / 67 MPa ISO 527
断裂伸长率 2.9 / 13.2 % ISO 527
无缺口简支梁冲击强度, +23°C 47 / 107 kJ/m² ISO 179/1eU
简支梁缺口冲击强度, +23°C 5.9 / 15 kJ/m² ISO 179/1eA
热性能干 / 已调节单位Test Standard
ISO数据
熔融温度, 10°C/min 220 / * °C ISO 11357-1/-3
热变形温度, 1.80 MPa 187 / * °C ISO 75-1/-2
热变形温度, 0.45 MPa 214 / * °C ISO 75-1/-2
1.5mm名义厚度时的燃烧性 HB / * class IEC 60695-11-10
Yellow Card 现存 是的 / * - -
电性能干 / 已调节单位Test Standard
ISO数据
相对漏电起痕指数 - / 550 - IEC 60112
其它性能干 / 已调节单位Test Standard
吸水性 8 / * % 类似ISO 62
吸湿性 2.6 / * % 类似ISO 62
密度 1240 / - kg/m³ ISO 1183
函数
应力-应变.  , Ultramid® B35G3 BK00564 (烘干), PA6-GF15, BASF
正割模量-应变.  , Ultramid® B35G3 BK00564 (烘干), PA6-GF15, BASF
拉伸模量-温度 , Ultramid® B35G3 BK00564 (烘干), PA6-GF15, BASF
典型数据
加工方法
注塑
供货形式
黑色
应用
汽车
地区供应
其他信息
注塑成型
PREPROCESSING
Pre/Post-processing, max. allowed water content: .15 %
Pre/Post-processing, Pre-drying, Temperature: 80 °C
Pre/Post-processing, Pre-drying, Time: 4 h

PROCESSING
injection molding, Melt temperature, range: 270 - 290 °C
injection molding, Melt temperature, recommended: 280 °C
injection molding, Mold temperature, range: 80 - 90 °C
injection molding, Mold temperature, recommended: 80 °C
injection molding, Dwell time, thermoplastics: 10 min
耐化学性
酸类
醋酸 (5g/100g) (23°C)
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com